Please use this identifier to cite or link to this item: https://ir.vidyasagar.ac.in/jspui/handle/123456789/1794
Full metadata record
DC FieldValueLanguage
dc.contributor.authorManna, A.-
dc.contributor.authorBhattacharya, R.-
dc.contributor.authorSaha, S.-
dc.contributor.authorSaha, S. C.-
dc.date.accessioned2018-01-20T00:44:05Z-
dc.date.available2018-01-20T00:44:05Z-
dc.date.issued2017-12-25-
dc.identifier.issn2350-0352 (print)-
dc.identifier.urihttp://inet.vidyasagar.ac.in:8080/jspui/handle/123456789/1794-
dc.description.abstractA simple chemical reduction route is followed to grow the CdSe nano structured materials at room temperature (30 0C). The growth time is kept 3 hours, 8 hours and 12 hours respectively to synthesize the material. The samples are characterized structurally, optically. The surface morphology of the samples are also studied. The result supports the formation of nanoparticle at 3 hours growth time. With the increase of growth time the nanoparticle structure changes to nanorod and is very prominent at 12 hours growth time. An increase in bandgap is also observed for the sample at higher growth times.en_US
dc.language.isoenen_US
dc.publisherVidyasagar Universityen_US
dc.relation.ispartofseriesJournal of Physical Sciences;JPS-v22-art10-
dc.subjectNanoparticles, Nanorods, Structural Properties, Surface Morphology, Bandgap.en_US
dc.subjectPhysicsen_US
dc.titleTransition from CdSe Nanoparticles to CdSe nanorods with Growth Timeen_US
dc.typeArticleen_US
Appears in Collections:Journal of Physical Sciences Vol.22 [2017]

Files in This Item:
File Description SizeFormat 
JPS-v16-art10.pdf363.66 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.